|Table of Contents|

High temperature deformation of reinforcement concrete beam bridges exposed to fire(PDF)

长安大学学报(自然科学版)[ISSN:1006-6977/CN:61-1281/TN]

Issue:
2009年01期
Page:
54-58
Research Field:
Publishing date:
2009-01-20

Info

Title:
High temperature deformation of reinforcement concrete beam bridges exposed to fire
Author(s):
ZHANG Gang1 HE Shuanhai1 GUO Qi2 SONG Yifan1
1. Key Laboratory for Bridge and Tunnel of Shaanxi Province, Changan University, Xian 710064, Shaanxi, China; 2. School of Civil Engineering, Xian University of Architecture and Technology, Xian 710055, Shaanxi, China
Keywords:
bridge engineering reinforcement concrete(RC) simply supported beam high temperature deformation nonlinear FEM
PACS:
TU375.1; TU352.5
DOI:
-
Abstract:
The temperature field distributions of rectangle section for RC simply supported beams exposed to the ISO834 standard fire are studied by numerical simulation program, and the influence laws of the covering layer thickness and load grades on the timeindependent deformation of RC beams at high temperature are presented. Based on mechanical balance principle and influence parameters, the model of inner force integration is proposed, and the nonlinear acceleration iteration equation is deduced with geometric progression. The simulation results indicate that the covering layer thickness has a great contribution to the deflection of RC simple beams, the timedependent curves for defleetion presents a nonlinear increase tendency with the raise of load grades; and its increase degree decrease with the increase of covering layer thickness; the increment of covering layer thickness is effective to fire resistance and control of deformation for RC simple beams. 8 figs, 10 refs.

References:

[1]余志武,王中强,史召锋.高温后新Ⅲ级钢筋力学性能的试验研究[J].建筑结构学报,2005,26(2):112116. YU Zhiwu,WANG Zhongqiang,SHI Zhaofeng.Experimental research on material properties of new Ⅲ grade steel bars after fire[J].Journal of Building Structures,2005,26(2):112116.
[2]Metin H.The effects of high temperature on compressive and flexural strengths of ordinary and highperformance concrete[J].Fire Safety Journal,2006,41(2):155163.
[3]余志武,丁发兴.圆钢管混凝土偏压柱的力学性能[J].中国公路学报,2008,21(1):4046. YU Zhiwu,DING Faxing.Mechanical behavior of concrete filled circular steel tubular columns under eccentric compression[J].China Journal of Highway and Transport,2008,21(1):4046.
[4]韩林海,杨华,霍静思,等.标准火灾作用后矩形钢 管混凝土柱剩余承载力的研究[J].工程力学,2002,19(5):7886. HAN Linhai,YANG Hua,HUO Jingsi,et al.Residual strength of concrete filled steel tubular columns with rectangular sections after exposure to standard fire[J].Engineering Mechanics,2002,19(5):7886.
[5]吴波,徐玉野.钢筋混凝土T形柱的耐火极限研究[J].土木工程学报,2007,40(3):3239. WU Bo,XU Yuye.Fire resistance of reinforced concrete columns of Tshaped cross section[J].China Civil Engineering Journal,2007,40(3):3239.
[6]Samantha F,Magdalena C,Christina H,et al.Thermal and structural behaviour of a fullscale composite building subject to a severe compartment fire[J].Fire Safety Journal,2007,42(3):183199.
[7]张岗,任伟,贺拴海,等.箱梁水化热温度场时效模式及时变应力场[J].长安大学学报:自然科学版,2008,28(4):5156. ZHANG Gang,REN Wei,HE Shuanhai,et al.Time dependent effect on hydration heat temperature and stress field for concrete box girder[J].Journal of Changan University:Natural Science Edition,2008,28(4):5156.
[8]张岗,贺拴海,宋一凡,等.火灾高温下钢筋混凝土梁桥非线性计算方法[J].西安建筑科技大学学报:自然科学版,2008,40(3):317322. ZHANG Gang,HE Shuanhai,SONG Yifan,et al.Nonlinear computation method for simply supported beam of reinforcement concrete exposed to fire[J].Journal of Xian Architecture and Technology:Natural Science Edition,2008,40(3):317322.
[9]张岗,贺拴海,宋一凡.混凝土箱梁水化热温度损伤修正耦合方法[J].交通运输工程学报,2008,8(1):5460. ZHANG Gang,HE Shuanhai,SONG Yifan.Updating coupling method of hydration heat temperature damage for concrete box girder[J].Journal of Traffic and Transportation Engineering,2008,8(1):5460.
[10]张岗,贺拴海,宋一凡,等.钢筋混凝土梁桥火灾安全评价[J].安全与环境学报,2008,8(3):153157. ZHANG Gang,HE Shuanhai,SONG Yifan,et al.Safety evaluation for reinforcement concrete girders exposed to fire[J].Journal of Safety and Environment,2008,8(3):153157.

Memo

Memo:
-
Last Update: 2009-01-20